PolyOne Lubri-Tech™ PC-30GF/15T Polycarbonate (PC)
Subcategory: Polycarbonate; Thermoplastic
Material Notes: Lubri-Tech™ Lubricated and Wear-Resistant Compounds have been specifically formulated to be self-lubricating materials, offering low coefficient of friction and improved wear resistance properties. These materials combine the unique benefits of internal lubricants such as PTFE, silicone and molybdenum disulfide with a wide array of base engineering resins. Lubri-Tech compounds have been demonstrated to reduce friction, noise, vibration, heat buildup and improve product durability.Description/Features: - PC (Polycarbonate)
- 30% Glass Reinforced
- 15% PTFE
Applications: - Low Friction
- Wear Resistance
- Noise Reduction
- Gears
- Pulleys
- Rollers
- Bearings
Processing Method: Injection Molding Information provided by PolyOne Corporation
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Coefficient of Friction
- Coefficient of Friction, Static
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|