PolyOne Elastamax® XL-2055 Thermoplastic Elastomer - TPO
Subcategory: Elastomer, TPE; Thermoplastic; Olefinic TPE
Material Notes:
Description/Features: - General Purpose Thermoplastic Elastomer
- UV Stabilized
Applications: Market: - Building and Construction
- Industrial
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.