PolyOne Geon® 0860-xx02D Vinyl Compound - Wire & Cable
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: - UL 105°C
- Non-lead
- Transparent
- Excellent Surface Appearance
- CL2
- CL2R
- Flame Retardant
Applications: - Telecommunication Insulation
- Telecommunication Jacket
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Oxygen Index
- Melt Temperature
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|