PolyOne Geon® 124A Polyvinyl Chloride Homopolymer (PVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: - Low molecular weight resin providing faster fusion characteristics
- Good chemical foamability for producing medium to high density foams
- Good multi-purpose resin for a wide range of end uses
- Good dispersability for easier plastisol preparation
Applications: - For med/high density foam (45 lbs/cu.ft+) or solid applications
- where good physical properties at lower temperatures are required
- Spread Coating
- Slush and Rotational Molding
- Dip Coating and Molding
- General plastisol formulations
- Solids and Foams
Dispersion Polymerization ProcessDisclaimer: Note: Plastisol Formulation F1 consists of 100 parts of this resin + 60 parts DOP. Note: Plastisol Formulation F2 consists of 100 parts of this resin + 57 parts DOP + 3 parts ESO + 2 parts Synpron® 940. Note: The values set forth represent "typical" values and PolyOne Corporation, therefore, makes no representation that the material in any particular shipment will conform to the listed properties. Manufacturing Location: This resin is produced at PolyOne's Pedricktown, NJ facility, which is ISO 9002 certified. Packaging: This resin is shipped in multi-wall paper bags, net weight 50 lbs, 2500 lbs per pallet. Information shown on the package includes commercial identification number, lot and weight. Information provided by PolyOne Corporation.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|