|   PolyOne Geon® 1410XX8OFRD Vinyl Compound - Wire & Cable  Subcategory: Vinyl; Thermoplastic Material Notes: 
 UL 105 C wire & cable insulation compound. THHN,THWN,THW,MTW,UL STYLES 1015,1007 and NMB insulation.PolyOne First Choice
 Information provided by PolyOne Corporation. 
| | 
    | Available Properties |  
    | Specific GravityHardness, Shore ATensile Strength, YieldElongation at BreakVolume ResistivityBrittleness TemperatureOxygen IndexMelt TemperatureOven Aged - Retention of Elongation (ROE)Oven Aged - Retention of Tensile Strength (ROT)
 | 
 | 
 |  | | 