PolyOne Geon® 2020 LO-GC Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic; Polymer
Material Notes:
Geon® 2020 LO-GC is a glass clear pellet compound designed for water bottle and other low odor applications that require FDA sanctioned materials. Description/Features: - Transparent
- High Impact
- High Gloss
- Low taste and odor
Applications: - FDA (Food Contact)
- Bottles
Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Density
- Specific Gravity
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Transmission, Visible
- Melt Temperature
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|