PolyOne Geon® 2800 IND-BL-1 Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
A high gloss transparent rigid PVC Compound designed for Industrial Blow Molding applications. This Compound is specifically formulated for large clear blow molded parts. Description/Features: Applications: Processing Method: - Extrusion - Profile, Sheet, Foam, Blow Molding
Information provided by PolyOne Corporation.
| Available Properties |
- Density
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Melt Temperature
- Product Form
|
|
|
|