PolyOne Geon® 86851 Vinyl Compound - Flexible (FPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
General Purpose Clear PVC Compound with low level of UV inhibitor. Description/Features: Applications: - Floor Mats
- General Purpose
- Hose and Tubing
Processing Method: - Extrusion and Molding
- Extrusion-Sheet
Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Tear Strength
- Brittleness Temperature
- Melt Temperature
- Product Form
|
|
|
|