PolyOne Geon® 87018 Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: Applications: Processing Method: PolyOne First ChoiceDisclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. NOTE: Physical Properties were measured on flat cellular profiles with a 0.72 specific gravity natural compound. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Dart Drop Total Energy
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
|
|
|
|
| Property Data |