PolyOne Geon® 87263 Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: - Exterior-Weatherable Natural Base
- UL 94 V0
Applications: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Geon weatherable compounds contain pigments and ingredients that, along with processing conditions, contribute to the weathering performance of the PVC compounds. The weathering performance of unpigmented compounds or so-called natural compounds generally is inferior to pigmented compounds. Unpigmented weatherable compounds may also contain non-pigment ingredients which can interact unpredictably with pigments to produce unexpected weathering results. Therefore, in applications where processors or customers would like to use an unpigmented compound, or add their own pigment package, it is the customer’s responsibility to determine whether or not the weathering performance after pigmenting is acceptable in their specific end-use application. Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Dart Drop Total Energy
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Cell Classification D1784
- Cell Classification D4216
- Ease of Sizing
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|