PolyOne Geon® 87727-0284 Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: - Interior UV Stable
- Pearlescent Appearance
- Translucent
- Colorless
Applications: - Custom Profiles
- Capstock
- Vertical Blinds
Processing Method: Physical property testing was based on the Geon® 87727 Trans 0020. PolyOne First Choice Disclaimer: Note: The Cell Classification was determined using the notched Izod test with injection molded samples. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Dart Drop Total Energy
- Izod Impact, Notched
- CTE, linear 68°F
- Deflection Temperature at 1.8 MPa (264 psi)
- Flammability, UL94
- Melt Temperature
- Cell Classification D1784
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|