| Available Properties | 
   
    
    - Specific Gravity
 
- Linear Mold Shrinkage
 
- Hardness, Shore A
 
- Tensile Strength, Ultimate
 
- Elongation at Break
 
- Tear Strength
 
- Compression Set
 
- Brittleness Temperature
 
- Clash Berg Stiffness Temperature
 
- Melt Temperature
 
- Product Form
 
 
   |   
   |   
 | 
   | 
  
  