PolyOne Geon® B6DW2 Vinyl Compound - Flexible (FPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
A Flexible PVC Compound containing Antifungus agent and UV screener for Exterior applications provided appropriate pigments package. Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.