PolyOne Geon® R208AE TPE - PVC/NBR
Subcategory: Vinyl; Elastomer, TPE; Thermoplastic
Material Notes:
Description/Features: - Oil/Fat Resistant
- Enhanced Compression Set
- Enhanced Low Temperature Properties
- Abrasion Resistant
Applications: - Boots
- Shoe Soles
- Shoe Uppers
Market: Processing Method: Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength, Ultimate
- Elongation at Break
- Brittleness Temperature
- Melt Temperature
- Product Form
- Ross Flex - Cut Growth
|
|
|
|