PolyOne Geon® UV-SORB-1 Vinyl Compound - Rigid (RPVC)
Subcategory: Vinyl; Thermoplastic
Material Notes:
Caution: To be used as an additive only. Bottles produced from blends of OxyClear UV-SORB-1 are specifically designed for use where UV sensitive products are being packaged. Dependent on the base Oxy Compound used, they may be used for either food contact or general purpose applications. Generally, additions of 4% to 10 % by Polymer weight, are recommended in order to comply with FDA Status. Description/Features: - High Impact
- Transparent
- High Gloss
- UV Absorber
Applications: - FDA (Food Contact)
- Bottles
Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Density
- Specific Gravity
- Hardness, Rockwell R
- Hardness, Shore D
- Tensile Strength, Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|