PolyOne Geon® W1213 Vinyl Compound - Wire & Cable
Subcategory: Vinyl; Thermoplastic
Material Notes:
Description/Features: - UL Recognized Insulation per UL QMTT2
- UL 105°C
- THW
- THHN
- THWN
- UL recognized for THW-2, THWN-2 in Black color only
- Flame Retardant
Applications: Market: Processing Method: Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength, Yield
- Elongation at Break
- Brittleness Temperature
- Oxygen Index
- Melt Temperature
- Product Form
|
|
|
|