PolyOne Gravi-Tech™ GRV-NJ-110-W Polyamide, Metal Filled
Subcategory: Nylon; Thermoplastic; Polymer
Material Notes:
Nontoxic alternative to Lead (Pb), weighting and balancing applications, radiation shielding applications. Description/Features: - High Specific Gravity
- High Flow
- Rigid
- Polyamide Base Resin
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Izod Impact, Notched
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
|
|
|
|