PolyOne Lubri-Tech™ NL-30GF/15T Nylon 6/12, Glass Filled, PTFE Lubricated
Subcategory: Nylon; Thermoplastic; Nylon 612; Polymer
Material Notes:
Description/Features: - Glass Fiber Reinforced
- PTFE Lubricated
- UL 94 HB (HEM TEST)
Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Hardness, Rockwell R
- Tensile Strength, Ultimate
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Compressive Strength
- Izod Impact, Notched
- Volume Resistivity
- CTE, linear 68°F
- Thermal Conductivity
- Deflection Temperature at 0.46 MPa (66 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|