PolyOne Maxxam® FR JS8831-23 Polypropylene (PP)
Subcategory: Polypropylene; Thermoplastic
Material Notes:
Description/Features: - Specialty Polyolefin
- Flame Retardant
- Data and voice communication wire
- CL2
- Superior stability
- Can be foamed by chemical agent or by gas injection
Applications: - Telecommunication Insulation
- Power and Control Cable Insulation
Market: Processing Method: PolyOne First ChoiceDisclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Melt Flow
- Tensile Strength @ Yield
- Elongation at Break
- Dielectric Constant
- Dissipation Factor
- Oxygen Index
- Oven Aged - Retention of Elongation (ROE)
- Oven Aged - Retention of Tensile Strength (ROT)
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|