PolyOne Nymax® 1308 A HS Natural Nylon 6/6, Glass Filled
Subcategory: Nylon; Thermoplastic; Nylon 66; Polymer
Material Notes:
The Nymax® Series of nylon 6/6 compounds have been specifically developed to deliver outstanding performance in a wide range of application areas. These materials are available with a broad range of fillers, glass reinforcement levels, and impact modifiers depending upon grade selected and have been formulated to offer ease of processing in most standard thermoplastic processing equipment. Description/Features: - Nylon 6/6 Compound
- Impact Modified
- Heat Stabilized
- Natural
Applications: Market: - Automotive
- Building and Construction
- Industrial
- Consumer Goods
Processing Method: Molded Test Bars: (Dry as Molded;PolyOne First Choice Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Filler Content
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength @ Yield
- Elongation at Break
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Deflection Temperature at 1.8 MPa (264 psi)
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|