PolyOne PolyAdd™ 1901-T Antiblock PEC Antiblock Additive Concentrate, Talc Filled
Subcategory: Additive/Filler for Polymer; Polymer
Material Notes:
1901-T is a heavily loaded concentrate for use where freedom from blocking is important. The talc used in this concentrate has been specifically developed by the producer as an antiblock additive. Its performance should be very similar to the performance of equal loadings of diatomaceous earth. Description/Features: Market: Processing Method: Note: Because of the high surface area of the antiblock additive, with certain minor resin additives, this concentrate can discolor after long storage times. Caution is advised to use 1901-T on a first in, first out basis to prevent discoloration. This concentrate is acceptable for FDA applications depending on end use. Information provided by PolyOne Corporation.
| Available Properties |
- Melt Flow
- Additive
- Base Resin
- Loading
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|