PolyOne Stat-Tech™ PS-NX 102902 CM Black Polybutylene Terephthalate (PBT)
Subcategory: Polyester, TP; Polybutylene Terephthalate (PBT); Thermoplastic
Material Notes:
Preliminary Data SheetPolyOne First Choice Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched
- Volume Resistivity
- Surface Resistivity per Square
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Product Form
|
|
|
|
| Property Data |