PolyOne Syncure™ S1016A Cross-Linked Polyethylene (XLPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
Moisture Crosslinkable Polyethylene Compound. Available as Base Resin component for PolyOne Syncure System. Market: Tensile, Elongation, Deformation, Hot Creep, and Gel measured on a 95 phr S1016A / 5 phr S1000B system; and cured for 6 hours in water at 90 degree C. Modulus measured on a 95 phr S1016A / 5 phr S1037B system. Pellet appearance is 1/8" cylindrical. PolyOne First Choice Information provided by PolyOne Corporation.