PolyOne Syncure™ S1044B Cross-Linked Polyethylene (XLPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
Available as Catalyst Masterbatch component for PolyOne Syncure System. Description/Features: Market: Gel values are >70, and were measured on a 90 phr S1054A / 10 phr S1044B Syncure System; and cured for 8 hours in steam. Pellet appearance is 1/8" Black Beads. PolyOne First Choice Information provided by PolyOne Corporation.