PolyOne Syncure™ System S100BL Cross-Linked Polyethylene (XLPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
Description/Features: - UL Bulletinized
- Silane grafted, two-step, moisture crosslinkable polyethylene system
- UL 90°C
- XHHW-2
- RHH
- RHW-2
- SIS
- USE-2
- Weatherable Grade
- Black
- Sunlight Resistant
- Flame Retardant
Applications: - Power and Control Syncure System
- Building Wire Syncure System
Market: Processing Method: PolyOne First ChoiceDisclaimer: STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap. NOTE: The above represents Typical Properties measured on 14 AWG with 30 mil wall. Information provided by PolyOne Corporation.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|