PolyOne Syncure™ System S112BL Cross-Linked Polyethylene (XLPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
Description/Features: - CSA listed Syncure System
- CSA 90°C
- Silane grafted, two-step, moisture crosslinkable polyethylene system
- 6 AWG and larger
- RW-90 and RWU-90 for outdoors
- Weatherable Grade
Applications: - Building Wire Syncure System
Market: Processing Method: PolyOne First ChoiceDisclaimer: STORAGE AND HANDLING: Use within 48 hours once package is open to avoid self-curing and scrap. Information provided by PolyOne Corporation.