PolyOne Syncure™ V0022G Cross-Linked Polyethylene (XLPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
Available as Flame Retardant Catalyst Masterbatch component for PolyOne Syncure System. Description/Features: Market: Gel, Torque, and Dispersion were measured on a 100 phr S1025A / 20 phr V0022G Syncure System. Cured for 6 hours in water at 90ºC for Gel test. Torque is > 1400. Dispersion is Visual. Pellet appearance is 1/8" round. PolyOne First Choice Information provided by PolyOne Corporation.
| Available Properties |
|
We're sorry, but our sources do not report any other information for this material.
|
|
|
|
| Property Data |