PolyOne Synprene® IT 37-035 Thermoplastic Elastomer - SBC, Mineral Filled
Subcategory: Elastomer, TPE; Thermoplastic; Styrenic TPE; Polymer
Material Notes:
Description/Features: - Multi-Purpose Thermoplastic Elastomer
- Mineral Filled
- UV Stabilized
Applications: Market: Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Tear Strength
|
|
|
|