PolyOne Synprene® IT 454 Thermoplastic Elastomer - SBC
Subcategory: Elastomer, TPE; Thermoplastic; Styrenic TPE
Material Notes:
Description/Features: - Multi-Purpose Thermoplastic Elastomer
Applications: - General Purpose
- Cove Base
- Interior
Market: - Automotive
- Consumer Goods
- Building and Construction
Processing Method: PolyOne First ChoiceInformation provided by PolyOne Corporation.