PolyOne Synprene® IT 62-002 BLACK 2001 Thermoplastic Elastomer - SBC
Subcategory: Elastomer, TPE; Thermoplastic; Styrenic TPE
Material Notes:
Description/Features: - Over-Molding Grade
- UV Stabilized
Applications: Multi-Purpose Processing Method: Injection Molding Information provided by PolyOne Corporation
| Available Properties |
- Specific Gravity
- Linear Mold Shrinkage
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Break
- Tear Strength
|
|
|
|