PolyOne Synprene® RT-3965 Thermoplastic Elastomer - SBC
Subcategory: Elastomer, TPE; Thermoplastic; Styrenic TPE
Material Notes:
Description/Features: - High Performance Thermoplastic Elastomer
- UV Stabilized
- Natural
Applications: Market: - Automotive
- Building and Construction
- Consumer Goods
- Industrial
Processing Method: - Injection Molding
- Extrusion
PolyOne First ChoiceInformation provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore A
- Tensile Strength @ Yield
- Elongation at Break
- Rebound
- Tear Strength
- Compression Set
- Brittleness Temperature
|
|
|
|