PolyOne VVO® 2-L Brown Coarse Vulcanized Vegetable Oil
Subcategory: Additive/Filler for Polymer
Material Notes:
Description/Features: - Plasticizer
- Prepared Rubber Additive
PolyOne First ChoiceDisclaimer: Storage Stability: In excess of one year when stored under proper conditions in original sealed container. Information provided by PolyOne Corporation.