PolyOne® CPE UV Res. Nat 1240 Chlorinated Polyethylene (CPE)
Subcategory: Polyethylene; Thermoset
Material Notes:
An excellent choice for low-voltage power-and-cable control cables, this filled, flexible thermoplastic CPE jacketing compound offers wire and cable manufacturers the advantages of thermoplastic extrusion processing without the need to invest in continuous vulcanization (CV) equipment. CPE 30-11 REV 2 is excellent for larger-diameter cable. This compound passes testing for heat/shock resistance, which requires cable to withstand being bent and twisted without cracking or showing stress. Good moisture, oil, and electrical properties. Applications include power-and-control cable for fossil-fuel and co-generation plants. Applications: - Power and Control Cable Jacket
Market: PolyOne First ChoiceDisclaimer: Note: Typical processing temperatures range between 320°-390°F depending upon screw design. Contact Technical Service for recommendation for specific equipment. Note: Pre-drying is recommended for 8-24 hours at 175°-185°F. NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Specific Gravity
- Hardness, Shore D
- Tensile Strength @ Yield
- Elongation at Break
- Tensile Modulus
- Oxygen Index
- Appearance
- Heat Shock, 1 hr @ 150° C
- Immersion- Elo. variation from Orig.
- Immersion- TS variation from Orig.
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|