So.F.TeR Forprene® 6E0 001 D60 Thermoplastic Elastomer - TPV
Subcategory: Elastomer, TPE; Thermoplastic
Material Notes:
Chemistry: Thermoplastic Elastomer - TPV Description/Features: Multi-Purpose Thermoplastic Elastomer, Natural Market: Automotive, Building and Construction, Consumer Goods, Industrial Applications: Multi-Purpose Processing Method: Extrusion, CoExtrusion Information provided by So.F.TeR Corporation.
| Available Properties |
- Density
- Hardness, Shore D
- Tensile Strength @ Break
- Elongation at Break
- 100% Modulus
- 300% Modulus
- Graves Tear Strength
|
|
|
|