PolyOne Geon® 1650-xx06FRD Vinyl Compound - Wire & Cable
Subcategory: Vinyl; Thermoplastic
Close Analogs: This product is no longer a part of the PolyOne standard product line.
Material Notes:
Chemistry: Vinyl Compound - Wire & Cable Description/Features: UL 75°C, CMR, CL2R, Accordance with National Electric Codes 800, 760, and 725, Passes UL 1581 Vertical Tray Burn, Flame Retardant Market: Wire & Cable Applications: Telecommunication Jacket Processing Method: Extrusion Coating Disclaimer: NOTE: Typical Properties of Molded Slab (0.075"); Not to be Construed as Specifications. Information provided by PolyOne Corporation.
| Available Properties |
- Density
- Hardness, Shore A
- Tensile Strength @ Break
- Elongation at Break
- Tensile Modulus
- Volume Resistivity
- Brittleness Temperature
- Oxygen Index
- Melt Temperature
- Oven Aged - Retention of Elongation (ROE)
- Oven Aged - Retention of Tensile Strength (ROT)
- Product Form
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|