Haysite 24500 Vinyl Ester BMC, 20% Glass Reinforced
Subcategory: Vinyl Ester; Polyester, TS; Thermoset; Polymer
Key Words: Haysite BMC
Material Notes: The 24500 series bulk molding compound offers good mechanical performance and excellent resistance to corrosive agents. This grade is formulated with a vinyl ester resin system and can be compression, transfer, or injection molded.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Maximum Service Temperature, Air
|
|
|
|