Haysite 48600 Polyester SMC, 30% Glass Reinforced
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Haysite SMC
Material Notes: The 48600 series sheet molding compound is formulated with a high temperature resin system (180º C). Designed for compression molding, this grade offers excellent retention of physical and electrical properties after exposure to elevated temperatures.