Haysite 54500 Polyester SMC, 35% Glass Reinforced
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Haysite SMC
Material Notes: A high strength fiberglass reinforced thermoset polyester compound formulated for injection, compression, or transfer molding. This material exhibits excellent electrical and mechanical properties, and has a UL94 Flame Class V-0.
| Available Properties |
- Density
- Water Absorption
- Linear Mold Shrinkage
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
- Maximum Service Temperature, Air
|
|
|
|