Haysite ULTRATRAC® H950 Glass Reinforced Polyester Sheet, Electrical Grade
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Haysite Sheet
Material Notes: This new generation of high performance material meets or exceeds all requirements for NEMA GPO-2 or GPO-3. ULTRATRAC ® H950 is recognized by U.L. as a 94V-0 material and offers greater arc and track protection with no increase in cost. Testing at an independent laboratory shows H950 to be non- toxic as defined by MIL M-14H. Excellent flame resistance and low smoke generation is also characteristic of this material. ULTRATRAC® H950 carries a U.L. thermal recognition of 160ºC electrical/150ºC mechanical. This is the highest rating ever assigned to a flame retardant glass polyester laminate. Applications are typical for GPO-3 materials, but also include components for transportation applications where flame, smoke, and toxicity is of great concern.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Notched
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Arc Resistance
- Comparative Tracking Index
- Maximum Service Temperature, Air
- UL RTI, Electrical
- UL RTI, Mechanical with Impact
- UL RTI, Mechanical without Impact
- Flammability, UL94
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|