Haysite HTF Glass Reinforced Polyester Sheet, Electrical Grade
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Haysite Sheet
Material Notes: This grade exhibits excellent flexibility and retention of electrical properties at elevated temperatures. HTF is an IEEE 200ºC Class N material and is part of numerous U.L. recognized 220ºC Class R insulation systems (U.L. File #E83907). Applications include layer and core insulation for dry type transformers.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Notched
- Dielectric Constant, Low Frequency
- Dielectric Strength
- Dissipation Factor, Low Frequency
- Arc Resistance
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|