Haysite H260 Polyester Laminate
Subcategory: Composite SMC; Polyester, TS; Thermoset
Key Words: Haysite Sheet
Material Notes: Solder Pallet and Work Holder Sheet An advanced composite that is high temperature resistant and high strength with semi-conductive properties. Engineered for use as wave and reflow solder pallet material, it may be used as dedicated or adjustable flow solder carriers as well as surface mount pallets. Standard color is blue/grey. Available thicknesses from 1/8" to 1/2" and 4mm to 12mm. Sheet sizes are 36" X 72" and 48" X 60", special thicknesses and custom sheet sizes are available.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Modulus
- Flexural Yield Strength
- Compressive Yield Strength
- Shear Strength
- Izod Impact, Notched
- Surface Resistance
- Maximum Service Temperature, Air
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|