Haysite Thermalate® H330 Glass Mat Reinforced Polyester Laminate
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Fiberglass
Material Notes: Platen Insulation. A thermoset insulation material with exceptional property retention at operating temperatures up to 550 F. Demonstrating superior compressive strength at high temperature, this grade provides extended use and greater maintenance and energy savings. Standard color is orange.
| Available Properties |
- Water Absorption
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- CTE, linear 20°C
- Thermal Conductivity
- Maximum Service Temperature, Air
|
|
|
|