Haysite H-193 Corrosion Resistant Polyester/Glass Sheet
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Fiberglass; Haysite Sheet
Material Notes: A fiber glass reinforced thermoset polyester sheet having good corrosion resistance to numerous acids and alkalis. This material also exhibits a high level of flame retardancy and low smoke generation. Typical applications are fume hood liner and weir panels for waste water treatment. Standard color is white. Extensive data covering resistance to specific chemicals is available upon request.
| Available Properties |
- Density
- Water Absorption
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Arc Resistance
- Flammability, UL94
|
|
|
|