Haysite HCR-197 Corrosion Resistant Polyester/Glass Sheet
Subcategory: Composite SMC; Polyester, TS; Thermoset; Polymer
Key Words: Fiberglass; Haysite Sheet
Material Notes: A fiber glass reinforced thermoset polyester sheet using ATLAC® 382 Bisphenol-A Fumarate in the resin matrix. Standard color is light yellow. Additional data covering resistance to specific chemicals is available upon request. Atlac® is a registered trademark of Reichhold Chemical, Inc.
| Available Properties |
- Density
- Water Absorption
- Hardness, Barcol
- Tensile Strength, Ultimate
- Flexural Yield Strength
- Compressive Yield Strength
- Izod Impact, Notched
- Dielectric Strength
- Arc Resistance
|
|
|
|