Celanese Celstran® PP-GF40-03 40% Long Glass Fiber Reinforced Polypropylene
Subcategory: Polypropylene; Thermoplastic; Polymer
Material Notes: Description: 40% long glass fiber reinforced, chemically coupled, heat stabilized, polypropylene Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|