Celanese Celstran® PA6-GF50-03 50% Glass Reinforced UV and Heat Stabilized Nylon 6
Subcategory: Nylon; Thermoplastic; Nylon 6; Polymer
Material Notes: Description: 50% glass reinforced, UV and Heat stabilized, Nylon 6 Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength at Break
- Elongation at Break
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Charpy Impact, Notched
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|