Topas® 8007F-04 Cyclic Olefin Copolymer Film
Subcategory: Thermoplastic; Polymer; Film
Material Notes: Classic extrusion grade for pharmaceutical, medical and food packaging applications. Mainly used in coextruded cast film applications, e.g. blister film. Provides excellent clarity, high stiffness/modulus, exceptional water vapor barrier properties and good thermoformability. Complies with USP Class VI and FDA as well as European Food Contact Directive. Migration or use limitations may apply.Information provided by Topas Advanced Polymers.
| Available Properties |
- Density
- Water Absorption at Saturation
- Moisture Vapor Transmission
- Oxygen Transmission
- Thickness
- Melt Flow
- Film Tensile Strength at Break, MD
- Film Tensile Strength at Break, TD
- Film Elongation at Break, MD
- Film Elongation at Break, TD
- Tensile Modulus
- Elmendorf Tear Strength MD
- Elmendorf Tear Strength TD
- Dart Drop Test
- Transformation Temperature, Tg
- Haze
- Gloss
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|