Topas® 5013 Cyclic Olefin Copolymer
Subcategory: Thermoplastic; Polymer
Close Analogs: Formerly a Ticona product
Material Notes: Description: Clear standard grade with a HDT/B of 130C. This grade is characterized by high flow and excellent optical properties. Recommended for applications such as precision optics, optical storage media, etc. where exceptional surface replication, and very low birefringence are a must. Complies with USP Class VI, and FDA Conditions of Use "A" thru "H" Data provided by Ticona & Topas Advanced Polymers, Inc.
| Available Properties |
- Density
- Water Absorption at Saturation
- Melt Flow
- Tensile Strength, Yield
- Elongation at Yield
- Tensile Modulus
- Poissons Ratio
- Charpy Impact Unnotched
- Charpy Impact, Notched
- Volume Resistivity
- Dielectric Constant
- Comparative Tracking Index
- CTE, linear 20°C
- CTE, linear 20°C Transverse to Flow
- Deflection Temperature at 0.46 MPa (66 psi)
- Refractive Index
- Haze
- Transmission, Visible
- Abbe Number
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|