Celanese Celanese® 6030UV High Impact, UV Stabilized Nylon 6/6
Subcategory: Nylon; Thermoplastic; Nylon 66
Material Notes: Description: Nylon 6030 UV is a high impact, UV stabilized nylon 6/6 which utilizes a UV stabilizer package to provide excellent UV stability. Data provided by Ticona.
| Available Properties |
- Density
- Linear Mold Shrinkage
- Tensile Strength, Yield
- Tensile Strength @ Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Modulus
- Izod Impact, Notched (ISO)
- Charpy Impact, Notched
- Izod Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Injection Pressure
- Back Pressure
- Screw Speed
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|