Celanese Celanex® 2025 Copolyester
Subcategory: Polyester, TP; Thermoplastic
Material Notes: Description: Celanex 2025 is a mid IV, unfilled, tough copolyester suitable for extrusion or injection molding. The product has an excellent balance of processing and mechanical properties and features improved elongation. Data provided by Ticona.
| Available Properties |
- Density
- Tensile Strength, Yield
- Elongation at Break
- Elongation at Yield
- Tensile Modulus
- Flexural Modulus
- Flexural Strength
- Izod Impact, Notched (ISO)
- Izod Impact, Unnotched (ISO)
- Charpy Impact, Notched
- Melting Point
- Deflection Temperature at 0.46 MPa (66 psi)
- Deflection Temperature at 1.8 MPa (264 psi)
- Rear Barrel Temperature
- Middle Barrel Temperature
- Front Barrel Temperature
- Nozzle Temperature
- Melt Temperature
- Mold Temperature
- Drying Temperature
- Dry Time
- Back Pressure
|
|
|
|
| Property Data |
This page displays only the text
of a material data sheet.
To see MatWeb's complete data
sheet for this material (including
material property data, metal
compositions, material suppliers,
etc), please click the button below. |
|
|
|
|
|